Supraduro SN 75
Supraduro SN 75 is a hemihydrate formulated plaster used in ceramics to produce working moulds for the slip casting tableware and sanitaryware.
Benefits
Fine particle size
High absorption capability
Stable workability
Supraduro SN 75 is a hemihydrate formulated plaster used in ceramics to produce working moulds for the slip casting tableware and sanitaryware.
Fine particle size
High absorption capability
Stable workability
Chemical Properties | |
---|---|
Chemical Composition | CaSO4.½H2O |
Chemical Name | Calcium Sulphate Hemihydrate |
Colour | off-white |
Minimum gypsum purity % | >92 |
Mechanical Properties | |
---|---|
Dry Compressive Strength (MPa) | >10 |
Flexural Strength (MPa) | >4.2 |
Setting Parameters | |
---|---|
Final setting time (minutes) | < 30 |
Initial setting time (minutes) | 8 - 12 |
Linear Expansion (%) | <0.2 |
Vicat Ring Fluidity (cm) | 19 - 23 |
Physical Properties | |
---|---|
Loose bulk density (kg/m³) | 620 - 720 |
Particle Size (% weight retained) |
< 6.0% at 63 µm < 1.0% at 90 µm |
Plaster to Water Ratio | |
---|---|
Plaster to water mix ratio (by weight) | 100/74 |
Plaster to Water Ratio (by weight) | 1.35:1 |
Water to plaster ratio ( by weight) | 74% |
The recommended plaster to water ratio is 1.35:1. The product can be used between 1.35:1 and 1.43:1, with a mixing time of approx. 2 to 4 minutes, depending on batch size. Mixing utensils should always be clean and free from set plaster. Use distilled water only. For consistent results, attention must be given to the correct proportioning and mixing of the plaster and water. Add the weighed quantity of plaster slowly into the measured volume of water and allow to soak. Do not mix fresh plaster with that which has been mixed for some time previously. Changes to plaster to water ratio will influence product performance, particularly setting time, strength and absorption capability.